MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Algoflon® G10 PTFE, Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Bronze Filled

Material Notes: Algoflon® G10 is a polytetrafluoroethylene (PTFE) virgin resin. This product has been developed as a PTFE resin for use in ASTM D4894-15, Type 1 applications. Algoflon® G10 is recommended for use in pyrotechnic applications.

Applications: Additive; Blending

Features: Chemical Resistant

Algoflon® G10 is classified as Type I Grade 1 resin in ASTM 04894, with the exception of Bulk Density.

NOTE: The data listed above fall with in the normal range of product properties, but they should not be used to establish specification limits nor be used alone as the basis of design.

SAFETY & HANDLING
Algoflon® G10 should be handled like other Algoflon® PTFE resins. When PTFE resins are heated to temperatures above 420°C, minor amounts of decomposition products, which may be harmful, are given off. Avoid inhalation of these fumes. Ovens and process equipment should be vented and adequate ventilation provided in the working area.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.13 - 2.18 g/ccASTM D4895
Bulk Density 0.500 g/ccASTM D4894
Particle Size 550 µmAverage
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 13.9 MPaASTM D4894
 
Descriptive Properties
AvailabilityEurope
ColorWhite
FormsPowder
ProcessingCompression Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4030 / 279830

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.