OKULEN® 1000 – AB – 5990 anti-microbial is a UHMW-PE Polymer. It has excellent anti-microbial protection. The protection range which has been measured is 99.99% against bacteria “Staphylococcus aureus ATCC6538P” and “Klebsiella pneumoniae ATCC 4352”. This grade is EU & FDA compliant for food industry. Properties: Excellent anti-microbial protection; water repellent; Good wear resistance; Very high notched impact strength; Very good sliding properties; EU 1935/2004 & 10/2011 – conform; FDA – conform Color: blue FN5990/similar RAL 5015 Range of applications: Hospital protection boards; Food industry Information provided by Okulen |