MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultradur® B 4300 G6 HR Unc. PBT, 30% Fiberglass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Ultradur B 4300 G6 HR Unc. is a hydrolysis resistant, 30% fiberglass reinforced PBT, exhibiting good balance of properties and flow.

Applications: Ultradur B 4300 G6 HR Unc. was developed for automotive connectors designed to meet USCAR Class III requirements.

Information provided by BASF.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.52 g/cc0.0549 lb/in³ISO 1183
Viscosity Test 105 cm³/g1.05 dl/gISO 1628
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 129 MPa18700 psiISO 527
Elongation at Break 3.7 %3.7 %ISO 527
Flexural Strength 199 MPa28900 psiISO 178
Flexural Modulus 7.80 GPa1130 ksiISO 178
Charpy Impact Unnotched 7.80 J/cm²37.1 ft-lb/in²ISO 179
Charpy Impact, Notched 1.40 J/cm²6.66 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 525 V525 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 223 °C433 °FISO 3146
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 275 °C482 - 527 °F
Mold Temperature 40.0 - 70.0 °C104 - 158 °F
 60.0 - 100 °C140 - 212 °Fupper end of range may be exceeded
Drying Temperature 100 - 120 °C
@Time 14400 sec
212 - 248 °F
@Time 4.00 hour
Moisture Content <= 0.040 %<= 0.040 %
Injection Pressure 3.45 - 10.3 MPa500 - 1500 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASF8906 / 254864

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.