MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Reynolds Encapso® K Water clear encapsulation rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Product Overview: Encapso™ K is a water clear encapsulation rubber that looks just like water and is ideal for a variety of encapsulation and display applications. How Does Encapso™ K Work? – Two clear liquids (Part A and Part B) are mixed together in equal amounts. The mixture is then poured around artificial flower stems or over an object. Encapso™ K cures to a soft rubber over night depending on casting thickness and conditions (see reverse side of this technical bulletin). When cured, Encapso™ K looks just like water and will last a long time.
Encapso™ K Advantages:
  • Non-Hazardous – No dangerous chemicals
  • Soft, Clear Rubber Lasts A Long Time
  • Easy To Use – Mix two liquids in equal amounts and pour
  • UV Resistant
  • Cures without generating any dangerous heat or fumes
  • Minimal Bubble Entrapment
  • Cures perfectly clear - Looks just like water
  • Cured rubber can be removed from object
Applications for Encapso™ K - This rubber is perfect for encapsulating artificial flower stems for creating lasting floral displays. You can also pour Encapso™ K around just about any inanimate object to encapsulate for display. You can also create a variety of display props and novelty items. Encapso™ K can be used to create water/pond effects for small scale model environments. Fully cured Encapso™ K can also be crumbled to look like broken glass, diamonds or ice. Add color to Encapso™ K with Silc Pig™ or Silc Pig™ Electric liquid color pigments.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.970 g/cc0.970 g/ccASTM D-1475
Viscosity 150 cP150 cPMixed; ASTM D-2393
Linear Mold Shrinkage <= 0.0010 cm/cm<= 0.0010 in/inASTM D-2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3333ASTM D-2240
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.17
@Frequency 100 Hz
3.17
@Frequency 100 Hz
Dielectric Strength 12.6 kV/mm319 kV/in
 
Processing PropertiesMetricEnglishComments
Cure Time 960 min16.0 hour
Pot Life 120 min120 minASTM D-2471
 
Descriptive Properties
ColorClear
Mix Ratio1A:1Bby volume
 1A:1Bby weight
Specific Volume28.6[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN160 / 296861

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.