MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

BEWiSynbra Circulum® GF-514p Expandable Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: Description: GF-514p is a flame retardant (FR) expandable polystyrene grade, containing graphite, with reduced thermal conductivity. Pentane is used as a blowing agent and a brominated polymeric flame retardant as an FR additive. The product is delivered in the form of spherical beads with a bulk density of about 0.6 g/cm3 and is available in 1100 kg octabins.

Applications: The properties of GF-514p make it suitable for the production of flame retardant light and heavy insulation board by block or shape moulding, in accordance with ISO EN 11925-2 class E.

Information provided by BEWi Synbra

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.600 g/cc0.0217 lb/in³
Storage Temperature 20.0 °C68.0 °F
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 0.130 MPa18.9 psi15 kg/m3; EN 12089
 0.200 MPa29.0 psi20 kg/m3; EN 12089
 0.260 MPa37.7 psi25 kg/m3; EN 12089
Compressive Strength  0.0700 MPa
@Strain 10 %
10.2 psi
@Strain 10 %
15 kg/m3; EN 826
 0.105 MPa
@Strain 10 %
15.2 psi
@Strain 10 %
20 kg/m3; EN 826
 0.140 MPa
@Strain 10 %
20.3 psi
@Strain 10 %
25 kg/m3; EN 826
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0290 W/m-K0.201 BTU-in/hr-ft²-°F20 kg/m3; EN 12667
 0.0290 W/m-K0.201 BTU-in/hr-ft²-°F25 kg/m3; EN 12667
 0.0310 W/m-K0.215 BTU-in/hr-ft²-°F15 kg/m3; EN 12667
 
Descriptive Properties
Raw material<0.1%Monomer level
 0.8-1.6 mmMain bead size distribution
 5.5-6.5%Pentane content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBEWS037 / 250846

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.