MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LNP™ STAT-KON™ Compound DD000P Polycarbonate (PC) (Asia)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP STAT-KON DD000P compound is based on Polycarbonate (PC) resin containing conductive carbon powder. Added features of this grade include: Electrically Conductive, Exceptional Processing.

Features: Exceptional Processing,Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ASTM D792
 1.23 g/cc0.0444 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.100 %0.100 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/in24hrs; ASTM D955
 0.0074 cm/cm0.0074 in/in24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0070 - 0.0090 cm/cm0.0070 - 0.0090 in/in24hrs; ASTM D955
 0.0084 cm/cm0.0084 in/in24hrs; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 49.0 MPa7110 psiASTM D638
 51.0 MPa7400 psiISO 527
Tensile Strength, Yield 57.0 MPa8270 psiASTM D638
 57.0 MPa8270 psiISO 527
Elongation at Break 9.9 %9.9 %ISO 527
 20.1 %20.1 %ASTM D638
Elongation at Yield 4.8 %4.8 %ASTM D638
 4.8 %4.8 %ISO 527
Tensile Modulus 2.75 GPa399 ksi50 mm/min; ASTM D638
 2.80 GPa406 ksi1 mm/min; ISO 527
Flexural Strength 78.0 MPa11300 psiISO 178
Flexural Modulus 2.40 GPa348 ksiISO 178
 2.75 GPa399 ksiASTM D790
Izod Impact Notched 234 J173 ft-lbASTM D256
Izod Impact, Unnotched 22.26 J/cm41.70 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 205 kJ/m²97.5 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 40.0 J29.5 ft-lbpeak; ASTM D3763
Impact Test 40.0 J29.5 ft-lbMultiaxial Impact; ISO 6603
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1000 - 1.00e+9 ohm1000 - 1.00e+9 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  66.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
36.7 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 66.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
37.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow  64.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
35.6 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 64.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
36.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 135 °C275 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 135 °C
@Thickness 3.20 mm
275 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 126 °C259 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 125 °C
@Thickness 3.20 mm
257 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 310 - 320 °C590 - 608 °F
Zone 3 320 - 330 °C608 - 626 °F
Melt Temperature 305 - 325 °C581 - 617 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81193 / 289140

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.