MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Versalis Edistir® N 3782 General Purpose Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: General purpose polystyrene with good flow and high heat resistance. N 3782 belongs to the third generation of Edistir® GPPS. The third generation of verbalism GPPS is characterized by a brighter, neutral appearance in line with more sophisticated market needs. Suggested for direct gassing extrusion of heavy gauge insulating boards (XPS) and in blends with high concentrations of clear SBS for improving clarity and stiffness of the sheets.

Applications: Designed for insulation panels (XPS), clear sheets and clear thermoformed packaging.

Information provided by Versalis.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.650 g/cc0.0235 lb/in³ISO 60
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Water Absorption <= 0.10 %
@Temperature 23.0 °C,
Time 86400 sec
<= 0.10 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/inISO 294/4
Melt Flow 7.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
7.5 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8080ISO 2039/2
Tensile Strength at Break 43.0 MPa6240 psi5 mm/min; ISO 527
Elongation at Break 1.6 %1.6 %5 mm/min; ISO 527
Tensile Modulus 3.25 GPa471 ksi1 mm/min; ISO 527
Flexural Strength 80.0 MPa11600 psi2 mm/min; ISO 178
Izod Impact, Notched (ISO)  1.50 kJ/m²
@Thickness 4.00 mm,
Temperature -30.0 °C
0.714 ft-lb/in²
@Thickness 0.157 in,
Temperature -22.0 °F
ISO 180/1A
 1.70 kJ/m²
@Thickness 4.00 mm,
Temperature 23.0 °C
0.809 ft-lb/in²
@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180/1A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 7.00e+15 ohm-cm>= 7.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.50e+15 ohm>= 1.50e+15 ohmIEC 60093
Dielectric Constant 2.5
@Frequency 50 Hz
2.5
@Frequency 50 Hz
IEC 60250
Dielectric Strength 70.0 kV/mm1780 kV/inIEC 60243
Dissipation Factor 0.00020
@Frequency 50 Hz
0.00020
@Frequency 50 Hz
IEC 60250
Comparative Tracking Index 400 V400 VSol.A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C38.9 µin/in-°FASTM D 696
Thermal Conductivity 0.170 W/m-K1.18 BTU-in/hr-ft²-°FISO 8302
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °F120°C/h, annealed; ASTM D 648
Vicat Softening Point  101 °C
@Load 5.10 kg
214 °F
@Load 11.2 lb
50°C/h; ISO 306/B
 106 °C
@Load 1.02 kg
223 °F
@Load 2.25 lb
50°C/h; ISO 306/A
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
Glow Wire Test 650 °C
@Thickness 1.60 mm
1200 °F
@Thickness 0.0630 in
IEC 60695-2-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENF9881 / 265575

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.