MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Cabot CSX™ 691 Specialty Carbon Black
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: CSX691 specialty carbon black has a low surface area and provides formulators an alternative to lamp black.

Key Applications: CSX691 specialty carbon black is an easy to disperse carbon black that can be used in a number of polymer and coatings applications, including:

  • Tinting black in plastics
  • Tinting black in liquid dispersions
  • Infrared (IR) opacifier in expandable polystyrene (EPS) foams
Product Features:
EPS Foams:
  • Morphology and surface chemistry are favorable for preparation and foaming of EPS foams
  • Good infrared absorption characteristics for lambda reduction provide improved thermal performance compared to white EPS
  • Designed to reduce interaction with other additives (e.g. flame retardants) in comparison with other carbon blacks
Tinting Black:
  • Low lot-to-lot variability facilitates consistent performance
  • Easy to disperse
  • Good tinting performance

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesOriginal ValueComments
Sulfur, S >= 0.40 %ASTM D-1619
 
Descriptive Properties
Iodine absorption15 mg/gASTM D-1510
OAN95 cc/100gASTM D-2414
Tint0.35ASTM D-3265

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCABOT117 / 315852

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.