MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® AVS4CC1 BK0888 PA66-GF35
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Vydyne AVS4CC1 BK0888 is part of Ascend's Anti-Vibration System portfolio. AVS4CC1 BK0888 is a 35% glass filled specialty compound that is specifically designed to provide an improvement in damping performance for critical NVH components without sacrificing the mechanical stiffness.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.42 g/ccDAM; ISO 1183
Water Absorption 1.1 %
@Temperature 23.0 °C,
Time 86400 sec
DAM; ISO 62
Moisture Absorption at Equilibrium 1.7 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 139 MPa50% RH; ISO 527-2
 199 MPaDAM; ISO 527-2
Elongation at Break 2.7 %DAM; ISO 527-2
 4.0 %50% RH; ISO 527-2
Tensile Modulus 9300 MPa50% RH; ISO 527-2
 11500 MPaDAM; ISO 527-2
Flexural Strength 198 MPa50% RH; ISO 178
 292 MPaDAM; ISO 178
Flexural Modulus 8800 MPa50% RH; ISO 178
 11200 MPaDAM; ISO 178
Poissons Ratio 0.34ISO 527-2
Izod Impact, Notched (ISO) 8.80 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 180/1A
 9.10 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 9.50 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 9.50 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 11.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 12.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched 58.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eU
 60.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 63.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eU
 64.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 77.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 79.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 8.80 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eA
 9.10 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 9.50 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 11.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 12.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 26.0 kV/mm
@Thickness 1.00 mm
50% RH; IEC 60243
 27.0 kV/mm
@Thickness 1.00 mm
DAM; IEC 60243
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 21.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 85.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
Melting Point 260 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 257 °CUnannealed, 50% RH; ISO 75-2/B
 260 °CUnannealed, DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 240 °CUnannealed, 50% RH; ISO 75-2/A
 247 °CUnannealed, DAM; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 280 - 310 °CInjection
Middle Barrel Temperature 280 - 310 °CInjection
Front Barrel Temperature 280 - 310 °CInjection
Nozzle Temperature 280 - 310 °CInjection
Melt Temperature 285 - 305 °CInjection
Mold Temperature 65.0 - 95.0 °CInjection
Drying Temperature 80.0 °C
Dry Time 4.00 hour
Moisture Content 0.15 %Injection
 
Descriptive Properties
AdditiveHeat Stabilizer
 Lubricant
Agency RatingsASTM, D4066 PA0100A5438
 ASTM, D6779 PA0100A5438
 ISO, 1043 PA66 GF35
AppearanceBlack
FeaturesFatigue Resistant
 Good Stiffness
 Good Strength
 Good Tensile Strength
 Heat Stabilized
 Lubricated
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific, South and Central America, Near East/Africa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE8484 / 320955

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.