MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Alfa Chemistry Materials Iron Nanorods
Categories: Metal

Material Notes:

Information provided by Alfa Chemistry Materials.

Vendors: Alfa Chemistry is an ISO 9001:2015 certified supplier of various materials, including: MOFs, coatings, nanomaterials, metals, polymers, carbon fibers, graphite, ceramics, glass, semiconductors, catalysts, carbon nanotubes, fullerene, COFs, molecular sieve, quantum dots, recycled plastics, photonic and optical materials, and magnetic materials, for customers worldwide. Alfa Chemistry also provides custom synthesis services for nearly all kinds of materials and chemicals. Learn more about Alfa Chemistry's high quality products at materials.alfachemic.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Molecular Weight 55.85 g/mol55.85 g/mol
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 608608MPa Microhardness
Modulus of Elasticity 211 GPa30600 ksi
Poissons Ratio 0.290.29
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000971 ohm-cm
@Temperature 20.0 °C
0.00000971 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 267 J/g115 BTU/lb
Heat of Vaporization 6338 J/g2727 BTU/lb
CTE, linear 11.8 µm/m-°C
@Temperature 25.0 °C
6.56 µin/in-°F
@Temperature 77.0 °F
Specific Heat Capacity 0.444 J/g-°C
@Temperature 25.0 °C
0.106 BTU/lb-°F
@Temperature 77.0 °F
Thermal Conductivity 80.4 W/m-K
@Temperature 25.0 °C
558 BTU-in/hr-ft²-°F
@Temperature 77.0 °F
Melting Point 1535 °C2795 °F
Boiling Point 2750 °C4980 °F
 
Descriptive Properties
Alfa Chemistry Materials CategoryMetals and Materials
AppearanceGray
CAS Number7439-89-6
EC Number231-096-4
Electronegativity1.8 Paulings
MDL NumberMFCD00010999
Molecular FormulaFe
Purity99%, 99.9%, 99.99%, 99.999%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

ZZALFA0961 / 269521

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.