MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Ertacetal® C ELS POM-C Polyoxymethylene
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Ertacetal® C ELS Polyoxymethylene POM-C shapes exhibit excellent electrical conductivity qualities, low moisture absorption, high strength and stiffness, and great machinability capabilities. This grade in particular is recommended for use in electrical and explosion sensitive applications.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.41 g/ccISO 1183-1
Water Absorption at Saturation 0.80 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 45ISO 2039-2
Tensile Strength 30.0 MPaISO 527-1/-2
Elongation at Break 8.0 %ISO 527-1/-2
Modulus of Elasticity 1.50 GPaISO 527-1/-2
Compressive Strength 14.0 MPa
@Strain 1 %
ISO 604
 37.0 MPa
@Strain 5.0 %
ISO 604
Charpy Impact Unnotched 89.0 kJ/m²ISO 179-1/1eU
Charpy Impact, Notched 5.00 kJ/m²ISO 179-1/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear 110 µm/m-°C
@Temperature 23.0 - 60.0 °C
 125 µm/m-°C
@Temperature 23.0 - 100 °C
Melting Point 173 °C10°C / min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 °C20,000 hours
Deflection Temperature at 1.8 MPa (264 psi) 105 °CISO 75-1/-2
Flammability, UL94 HB
@Thickness 3.00 mm
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

P1SM914 / 291071

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.