Product Description: RUBALOY 2530 is unique blend of 50% acrylonitrile (NBR) and 50% polyvinyl chloride (PVC) with 75% DINP oil. Rubaloy 2530 can be easily processed on conventional rubber mixing/compound machines, has excellent filler and plasticizer absorption properties, and can withstand elevated compounding temperatures. It provides substantial tensile strength considering the level of plasticizer. Rubaloy 2530 can be sulfur and peroxide cured. A slightly higher level of accelerators is recommended. Applications: RUBALOY 2530 can be used in a variety of rubber compounding applications such as: low hardness printing rolls, molded articles, low density foam, soft pipes, tubes, and hoses. Information provided by Akrochem Corporation |