MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Epoxies, Etc 20-1615 Water Clear Silicone Potting Compound
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: 20-1615 is a two component, room temperature curing silicone rubber compound. This silicone system is clear, odorless, and low in viscosity. 20-1615 is an excellent choice for potting electronic assemblies that require shock and vibration resistance. It also protects assemblies from moisture, ozone, chemicals and other environmental hazards.

Features:

  • Low viscosity
  • No exotherm during cure
  • Contains no solvents
  • Hydrolytic stability
  • Operating temperature -65 to +205?C
  • Easy 10:1 Ratio

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 g/cc1.03 g/cc
Viscosity 6000 cP6000 cPmixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040
Tensile Strength 6.55 MPa950 psi
Elongation at Break 120 %120 %
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.20e+15 ohm-cm1.20e+15 ohm-cm
Dielectric Constant 2.7
@Frequency 1000 Hz
2.7
@Frequency 1000 Hz
Dielectric Strength 19.7 kV/mm500 kV/in
Dissipation Factor 0.0040
@Frequency 1000 Hz
0.0040
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 329 µm/m-°C183 µin/in-°F
Thermal Conductivity 0.0173 W/m-K0.120 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 205 °C401 °F
Minimum Service Temperature, Air -65.0 °C-85.0 °F
Shrinkage 0.20 %0.20 %
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.401.40
 
Processing PropertiesMetricEnglishComments
Pot Life 240 min240 min
 
Descriptive Properties
ColorWater clear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFEPOX000 / 316677

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.