MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chemours Teflon™ AF 1601 Amorphous Fluoropolymer Solutions
Categories: Polymer; Thermoplastic; Fluoropolymer

Material Notes: Teflon™ AF is a family of amorphous fluoropolymers similar to other amorphous polymers in optical clarity and mechanical properties, including strength, but also perform like fluoropolymers in their performance over a wide range of temperatures, outstanding electrical properties, and chemical resistance. Teflon™ AF solutions are made of Teflon™ AF amorphous fluoropolymer dissolved in Fluorinert® FC-40. Products labeled AF 1601 and AF 1601 X are equivalent. Applications: low-refractive-index coating or covering for optical devices, optoelectronic devices.

Information provided by Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.78 g/ccASTM D792
Water Absorption <= 0.010 %
Brookfield Viscosity 190 - 220 cPIn Fluorinert® FC-40 @ 6 wt%.
Melt Flow 2.0 - 10 g/10 min
@Load 5.00 kg,
Temperature 225 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 1.60 - 13.8 MPa
@Temperature 220 °C
 25.4 - 28.4 MPa
@Temperature 23.0 °C
Elongation at Break 12.1 - 22.1 %
@Temperature 23.0 °C
ASTM D638
Tensile Modulus 1.60 GPaASTM D638
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 1.93ASTM D150
Dissipation Factor 0.00010 - 0.00020ASTM D150
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 155 - 165 °CASTM D3418
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.31ASTM D542
Transmission, Visible >= 95 %ASTM D1003
 
Descriptive Properties
Contact Angle with Water104ASTM D570
Critical Surface Energy15.7 Dynes/cm
Solubility in Fluorinert® FC40Up to 18 wt%23°C
Volume Coefficient of Thermal ExpansionASTM E831

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDU8776 / 268702

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.