MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Abhar Polymer Compounds APLSB01 Flame Retardant Cable Bedding Compound
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: APLSB01 is a thermoplastic, low smoke, halogen free, flame retardant cable bedding compound. This product provides good processing characteristics and physical properties. APLSB01 is used as bedding compound for XLPE insulation and HFFR sheathing.

Specification: Cables manufactured with APLSB01 according to standard technology meet industrial cable Specifications as per BS 6724 for bedding PABHARs.

Information provided by Abhar Polymer Compounds

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.48 - 1.52 g/ccASTM D792
Melt Flow 3.0 - 4.0 g/10 min
@Load 21.6 kg,
Temperature 150 °C
ASTM D1238
Storage Temperature <= 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 53 - 57ASTM D2240
Tensile Strength >= 11.0 MPaIEC 60811-1-1
Elongation at Break >= 140 %IEC 60811-1-1
Heat Distortion 30 %
@Temperature 80.0 °C
IEC 60811-3-1
 
Thermal PropertiesOriginal ValueComments
Smoke Density 10[%]; ASTM D 2843
Oxygen Index 33 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Zone 1 130 - 140 °C
Zone 2 140 - 145 °C
Zone 3 145 - 150 °C
Zone 4 150 - 155 °C
Die Temperature 160 - 165 °C
Head Temperature 160 - 165 °C
 
Descriptive Properties
Acid gas emission<10 µS/mmConductivity, IEC 60754-2
 >4.3P, IEC 60754-2
Flame spread test on single cables>5 mmIEC 60332-1
Halogen acid gas evolution0IEC 60754-1
Toxicity Index1.7NES 713

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PABHAR010 / 249443

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.