MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Phosphor bronze 10% Sn, UNS C52400, OS035 Temper, Flat Products & Wire
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: Nominal Grain Size 0.035 mm

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Butt Weld; Good Suitability – Gas Shielded Arc Welding, Spot Weld, Capacity for Being Cold Worked; Fair Suitability – Oxyacetylene Welding, Coated Metal Arc Welding, Seam Weld; Poor Suitability – Capacity for Being Hot Formed

Common Fabrication Processes: Bending; Blanking; Forming; Shearing

Typical uses: Expansion Plates for Bridges; Fittings; Heavy Bars and Plates

Applicable Specifications: Bar – ASTM B139/B139M, ASTM B103/B103M; Plate – ASTM B103/B103M; Rod – Welding AWS A5.15, ASTM B139/B139M, SAE J461, SAE J463; Shapes – ASTM B139/B139M; Sheet – ASTM B103/B103M; Strip – SAE J463, ASTM B103/B103M, SAE J461; Wire – ASTM B159/B159M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.77 g/cc0.317 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  455 MPa
@Thickness 2.03 mm
66000 psi
@Thickness 0.0800 in
 455 MPa
@Thickness 1.02 mm
66000 psi
@Thickness 0.0400 in
Elongation at Break  68 %
@Thickness 1.02 mm
68 %
@Thickness 0.0400 in
 70 %
@Thickness 2.03 mm
70 %
@Thickness 0.0800 in
Tensile Modulus 110 GPa16000 ksi
Modulus of Rigidity 41.4 GPa6000 ksi
Poissons Ratio 0.330.33Calculated
Machinability 20 %20 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000156 ohm-cm0.0000156 ohm-cm11% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.4 µm/m-°C
@Temperature 20.0 - 300 °C
10.2 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 4.18 W/m-K29.0 BTU-in/hr-ft²-°F
Melting Point 843 - 999 °C1550 - 1830 °F
Solidus 843 °C1550 °F
Liquidus 999 °C1830 °F
Annealing Point 482 - 677 °C900 - 1250 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 88.3 - 91 %88.3 - 91 %As Balance
Iron, Fe <= 0.10 %<= 0.10 %
Lead, Pb <= 0.050 %<= 0.050 %
Phosphorus, P 0.030 - 0.35 %0.030 - 0.35 %
Tin, Sn 9.0 - 11 %9.0 - 11 %
Zinc, Zn <= 0.20 %<= 0.20 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC52400x3 / 293007

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.