MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

SABIC LNP™ THERMOTUF™ Compound WF008NA Polybutylene Terephthalate (PBT)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: LNP THERMOTUF WF008NA compound is based on Polybutylene Terephthalate (PBT) resin containing 40% glass fiber. Added features of this grade include: High Modulus, Impact Modified, Good Metal Bonding Strength and Good Chemical Resistance suitable for Nano-Molding Technology (NMT) applications and Good Color Stability during anodizing process.

Features: Impact Modified,High Stiffness,Chemical Resistance,Good metal adhesion,Nano molding technology grade,Color Stability,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.61 g/cc0.0582 lb/in³ASTM D792
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Viscosity  17 cP
@Load 5.00 kg,
Temperature 250 °C
17 cP
@Load 11.0 lb,
Temperature 482 °F
MVR cc/10 min; ISO 1133
 32 cP
@Load 5.00 kg,
Temperature 275 °C
32 cP
@Load 11.0 lb,
Temperature 527 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0027 cm/cm0.0027 in/inSABIC method
Linear Mold Shrinkage, Transverse 0.0050 cm/cm0.0050 in/inSABIC method
Melt Flow  15 g/10 min
@Load 2.16 kg,
Temperature 275 °C
15 g/10 min
@Load 4.76 lb,
Temperature 527 °F
ASTM D1238
 43 g/10 min
@Load 5.00 kg,
Temperature 275 °C
43 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 155 MPa22500 psi5 mm/min; ISO 527
 156 MPa22600 psi5 mm/min; ASTM D638
Elongation at Break 3.2 %3.2 %5 mm/min; ASTM D638
 3.2 %3.2 %5 mm/min; ISO 527
Tensile Modulus 12.527 GPa1816.9 ksi1 mm/min; ISO 527
 12.8 GPa1860 ksi5 mm/min; ASTM D638
Flexural Strength 228 MPa33100 psibreak, 2mm/min; ISO 178
 236 MPa34200 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 11.1 GPa1610 ksi1.3 mm/min, 50 mm span; ASTM D790
 11.72 GPa1700 ksi2 mm/min; ISO 178
Adhesive Bond Strength 38.0 MPa5510 psi(TRI) , 5 mm/min, Type A; ISO 19095
Izod Impact Notched 132 J97.4 ft-lbASTM D256
 100 J
@Temperature -30.0 °C
73.8 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched 9.12 J/cm17.1 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 13.0 kJ/m²6.19 ft-lb/in²80*10*4; ISO 180/1A
 12.0 kJ/m²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 54.0 kJ/m²25.7 ft-lb/in²80*10*4; ISO 180/1U
Charpy Impact Unnotched 6.00 J/cm²28.6 ft-lb/in²ISO 179/2C
Charpy Impact, Notched 1.40 J/cm²6.66 ft-lb/in²ISO 179/2C
 1.30 J/cm²
@Temperature -30.0 °C
6.19 ft-lb/in²
@Temperature -22.0 °F
ISO 179/2C
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.96
@Frequency 1.90e+9 Hz
3.96
@Frequency 1.90e+9 Hz
SABIC method
 3.96
@Frequency 5.00e+9 Hz
3.96
@Frequency 5.00e+9 Hz
SABIC method
 3.97
@Frequency 1.10e+9 Hz
3.97
@Frequency 1.10e+9 Hz
SABIC method
Dissipation Factor  0.0090
@Frequency 5.00e+9 Hz
0.0090
@Frequency 5.00e+9 Hz
SABIC method
 0.010
@Frequency 1.90e+9 Hz
0.010
@Frequency 1.90e+9 Hz
SABIC method
 0.011
@Frequency 1.10e+9 Hz
0.011
@Frequency 1.10e+9 Hz
SABIC method
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  18.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
10.0 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 19.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
10.6 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow  60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 66.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
36.7 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 208 °C406 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 204 °C
@Thickness 6.40 mm
399 °F
@Thickness 0.252 in
unannealed; ASTM D648
 206 °C
@Thickness 3.20 mm
403 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 208 °C406 °FRate B/50; ASTM D1525
 221 °C430 °FRate A/50; ISO 306
UL RTI, Electrical 75.0 °C167 °FUL 746B
UL RTI, Mechanical with Impact 75.0 °C167 °FUL 746B
UL RTI, Mechanical without Impact 75.0 °C167 °FUL 746B
Flammability, UL94 HB
@Thickness 0.700 mm
HB
@Thickness 0.0276 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 255 - 275 °C491 - 527 °F
Zone 2 250 - 270 °C482 - 518 °F
Zone 3 250 - 270 °C482 - 518 °F
Melt Temperature 250 - 270 °C482 - 518 °FInjection Molding
Mold Temperature 100 - 160 °C212 - 320 °F
Drying Temperature 100 - 120 °C212 - 248 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Precipitation Temperature 40.0 - 60.0 °C104 - 140 °FHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82043 / 289990

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.