MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cabot CAB-O-SIL® ULTRABOND™ Fumed Silica
Categories: Other Engineering Material

Material Notes: Product highlights: CAB-O-SIL ULTRABOND fumed silica is our highest performing surface treated fumed silica. Compared to other polydimethylsiloxane (PDMS) treated silicas, CAB-O-SIL ULTRABOND fumed silica improves adhesives systems by reducing the viscosity in the application without compromising sag resistance. CAB-O-SIL ULTRABOND fumed silica is best suited for epoxy adhesives with loading levels greater than 5% and those that require high sag resistance and excellent storage stability.

Key applications: Structural adhesives for epoxy formulations in a wide range of industries:

  • Automotive
  • Aerospace
  • Construction
  • Electronics
  • Flooring
  • Wind bonding paste
Performance Features: In epoxy resins, CAB-O-SIL ULTRABOND fumed silica provides excellent sag resistance and storage stability compared to other PDMS treated silicas. Figure 1 shows the sag resistance in epoxy resin, as assessed by a Yield Stress measurement, upon manufacture, and after 28 days of accelerated aging at 60 °C. The epoxy resins containing CAB-O-SIL ULTRABOND fumed silica were shown to provide higher Yield Stress both initially and after aging than epoxies made with competitive PDMS treated silicas.

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Product FormPowder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCABOT104 / 315839

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.