MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Danquinsa DANTHANE® 125KG TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: DANTHANE_ 125KG is a polyester based, aromatic TPU, already colored in green. This TPU granule is best suitable for coatings and films, that must show high flexibility also at low temperatures. DANTHANE_ 125KG is mainly used at the production of green colored transport elements (transport and conveyor belt coatings).

Application: DANTHANE_ 125KG is applied at the hot melt coating of industrial textiles. The coated textiles are used for transport and drive sections. DANTHANE_ 125KG is favored used for sinter coatings of textiles. Concerning powder we refer to the type DANTHANE_ 125KG-Powder.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccDIN 53.479
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85DIN 53.505
Tensile Strength 25.0 MPaDIN 53.504
Elongation at Break 620 %DIN 53.504
100% Modulus 5.50 MPaDIN 53.504
200% Modulus 6.00 MPaDIN 53.504
300% Modulus 8.00 MPaDIN 53.504
Abrasion 30[mm³]; DIN 53.516
Compression Set 30 %
@Temperature 23.0 °C,
Time 252000 sec
DIN 53.517
 80 %
@Temperature 70.0 °C,
Time 86400 sec
DIN 53.517
 
Thermal PropertiesOriginal ValueComments
Melting Point 135 - 145 °CKofler
Softening Point 120 - 125 °CKofler
Glass Transition Temp, Tg -30.0 °CDSC; DIN 51.007
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
AspectGreen colored pearl granulecolor RAL 6005

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDANQ142 / 294562

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.