MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ ELCRIN™ WF006NAiQ Polybutylene Terephthalate (PBT)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: LNP ELCRIN WF006NAiQ is an iQ PBT based compound containing 30% glass for NMT application. Added features of this material include: >25% PCR, high metal bonding strength, and good chemical resistance.

Features: Post-Consumer Recycled (PCR) content,High Stiffness,Chemical Resistance,Good metal adhesion,Nano molding technology grade,Good dimensional stability,High Flow,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.48 g/cc0.0535 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Viscosity  9.0 cP
@Load 5.00 kg,
Temperature 250 °C
9.0 cP
@Load 11.0 lb,
Temperature 482 °F
MVR cc/10 min; ISO 1133
 19 cP
@Load 5.00 kg,
Temperature 275 °C
19 cP
@Load 11.0 lb,
Temperature 527 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm0.0020 - 0.0030 in/inSABIC method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0050 cm/cm0.0040 - 0.0050 in/inSABIC method
Melt Flow  12 g/10 min
@Load 5.00 kg,
Temperature 250 °C
12 g/10 min
@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
 24 g/10 min
@Load 5.00 kg,
Temperature 275 °C
24 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 111 MPa16100 psi5 mm/min; ISO 527
 113 MPa16400 psi5 mm/min; ASTM D638
Elongation at Break 2.6 %2.6 %5 mm/min; ISO 527
 2.7 %2.7 %5 mm/min; ASTM D638
Tensile Modulus 8.70 GPa1260 ksi1 mm/min; ISO 527
 8.80 GPa1280 ksi5 mm/min; ASTM D638
Flexural Strength 173 MPa25100 psi2 mm/min; ISO 178
 178 MPa25800 psi1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 7.40 GPa1070 ksi2 mm/min; ISO 178
 7.77 GPa1130 ksi1.3 mm/min, 50 mm span; ASTM D790
Adhesive Bond Strength 32.0 MPa4640 psi("T" treatment, shear type); ISO 19095
Izod Impact Notched 150 J111 ft-lbASTM D256
 110 J
@Temperature -30.0 °C
81.1 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched 9.10 J/cm17.0 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 14.5 kJ/m²6.90 ft-lb/in²80*10*4; ISO 180/1A
 11.0 kJ/m²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 51.0 kJ/m²24.3 ft-lb/in²80*10*4; ISO 180/1U
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.64
@Frequency 1e+10 Hz
3.64
@Frequency 1e+10 Hz
SABIC method
 3.65
@Frequency 1.10e+9 Hz
3.65
@Frequency 1.10e+9 Hz
SABIC method
 3.66
@Frequency 5.00e+9 Hz
3.66
@Frequency 5.00e+9 Hz
SABIC method
 3.69
@Frequency 1.90e+9 Hz
3.69
@Frequency 1.90e+9 Hz
SABIC method
Dissipation Factor  0.011
@Frequency 1e+10 Hz
0.011
@Frequency 1e+10 Hz
SABIC method
 0.013
@Frequency 5.00e+9 Hz
0.013
@Frequency 5.00e+9 Hz
SABIC method
 0.014
@Frequency 1.90e+9 Hz
0.014
@Frequency 1.90e+9 Hz
SABIC method
 0.015
@Frequency 1.10e+9 Hz
0.015
@Frequency 1.10e+9 Hz
SABIC method
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  24.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
13.3 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 24.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
13.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  82.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
45.6 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 86.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
47.8 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 201 °C394 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 206 °C
@Thickness 3.20 mm
403 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 165 °C329 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 172 °C
@Thickness 3.20 mm
342 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 245 - 275 °C473 - 527 °F
Zone 2 250 - 270 °C482 - 518 °F
Zone 3 250 - 270 °C482 - 518 °F
Melt Temperature 250 - 270 °C482 - 518 °FInjection Molding
Mold Temperature 100 - 160 °C212 - 320 °F
Drying Temperature 100 - 120 °C212 - 248 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Precipitation Temperature 40.0 - 60.0 °C104 - 140 °FHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80619 / 288566

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.