MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Kumho-Sunny Colorful-in™ PC-M PC
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: PC-M is injection a molding aesthetic resin. PC-M is a color creativity plan. PC-M can be used for high degree of color and semitransparent design. PC-M is mainly used in appearance items of household appliance, etc.

Information provided by Shanghai Kumho Sunny Plastics co, Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Maximum Moisture Content 0.0300.030
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
Melt Flow 30 g/10 min
@Load 5.00 kg,
Temperature 260 °C
30 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength 60.0 MPa8700 psiASTM D638
Flexural Strength 80.0 MPa11600 psiASTM D790
Flexural Modulus 2.30 GPa334 ksiASTM D790
Izod Impact, Notched 3.00 J/cm
@Thickness 3.20 mm
5.62 ft-lb/in
@Thickness 0.126 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FASTM D648
Vicat Softening Point 125 °C257 °FB; ASTM D1525
Flammability, UL94 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 250 - 260 °C482 - 500 °F
Middle Barrel Temperature 240 - 265 °C464 - 509 °F
Front Barrel Temperature 240 - 265 °C464 - 509 °F
Nozzle Temperature 240 - 250 °C464 - 482 °F
Melt Temperature 250 - 265 °C482 - 509 °F
Mold Temperature 85.0 - 95.0 °C185 - 203 °F
Drying Temperature 100 - 120 °C212 - 248 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Back Pressure 0.300 - 1.00 MPa43.5 - 145 psi
Screw Speed 40 - 55 rpm40 - 55 rpm
 
Descriptive Properties
Pencil HardnessHB500g, ASTM D2179

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKMSN014 / 280866

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.