MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Akrochem Antioxidant 60
Categories: Other Engineering Material

Material Notes: Product Description: Antioxidant 60 (2-mercapto-4(5)-methylbenzimidazole) is a non-discoloring and non-staining antioxidant for natural and synthetic rubbers, except polychloroprene. Protection against heat and oxygen aging is excellent, especially when combined with amine or phenol type antioxidant, wherein a synergistic effect yields results superior to those of the separate constituents. Antioxidant 60 acts as a metal deactivator when used synergistically with Antiozonant PD-1 (black compounds) or Antioxidant 1024 (non-black compounds).

Application: In addition to its antioxidant properties, Antioxidant 60 provides improved protection against rubber poisons, especially in combination with Antioxidant 33 or 235, or Antiozonants PD-1 or PD-2. It also imparts steam resistance to rubber compounds and has a brightening effect on transparent goods. In spite of its high melting point, Antioxidant 60 disperses readily in rubber mixes. It does have a slight retarding effect in sulfur cures and reduces modulus slightly. Maximum protection is provided in thiuram and dithiocarbamate curing systems containing little or no sulfur. For general applications, 0.6 - 1.5 phr Antioxidant 60 is used. For heat resistant thiuram cured compounds, 2 - 3 phr is used, or 1 - 2 phr in combination with 1 - 2 phr Antioxidant DQ, Antiozonant PD-1 or PD-2.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/cc
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 270 °C
 
Descriptive Properties
Appearanceyellow-white micro-granule (oil-treated)
Content0.015Oil

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH487 / 315405

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.