Transparent, FDA compliant, low melt flow for extrusion and injection molding Veradel® A-201 is a low melt flow general purpose amorphous PESU resin for extrusion injection molding. This transparent grade offers high heat deflection temperature, excellent toughness and dimensional stability and resistance to mineral acids. Other desirable properties include thermal stability, creep resistance and inherent flame resistance. Veradel® A-201 is FDA compliant and is approved for direct food contact. This grade was formerly marketed as Radel® A PESU. - Natural: Veradel® A-201 NT Applications: Appliance Components; Appliances; Automotive Electronics; Batteries; Business Equipment; Electrical Parts; Electrical/Electronic Applications; Food Service Applications; Industrial Applications; Microwave Cookware Features: Acid Resistant; Chemical Resistant; Creep Resistant; Flame Retardant; Food Contact Acceptable; General Purpose; Good Adhesion; Good Dimensional Stability; Good Thermal Stability; Good Toughness; High Heat Resistance; High Tensile Strength; Hydrolysis Resistant; Medium Flow; Medium Molecular Weight; Medium Rigidity Information provided by Solvay Specialty Polymers. |