MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Radici Radilon® D 40EP25ZW 7037 BL Polyamide 610
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610)

Material Notes: PA610 flexible, high viscosity extrusion grade. Toughened and plasticized, heat stabilized. Blue color. Suitable for extrusion of pipes, profiles, and cable jackets. Good impact resistance also at low temperatures. This grade is partially renewable sourced (60% of base polymer by weight.)

Information provided by Radici Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccDAM; ISO 1183
Water Absorption 2.0 %
@Thickness 2.00 mm,
Time 86400 sec
Immersion @ 23°C; ISO 62
Moisture Absorption 0.900 %
@Thickness 2.00 mm,
Temperature 23.0 °C
50% RH; ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 27.0 MPa50mm / min. Conditioned; ISO 527-2/1A
 30.0 MPa50mm / min. DAM; ISO 527-2/1A
Tensile Strength, Yield 24.0 MPa
@Strain 50 %
ISO 527-2/1A
 27.0 MPa
@Strain 50 %
ISO 527-2/1A
Elongation at Break >= 50 %5 mm / min. Conditioned; ISO 527-2/1A
 >= 50 %5 mm / min. DAM; ISO 527-2/1A
Tensile Modulus 380 MPa1mm / min. Conditioned; ISO 527-2/1A
 560 MPa1mm / min. DAM; ISO 527-2/1A
Flexural Strength 15.0 MPa2mm / min. Conditioned; ISO 178
 20.0 MPa2mm / min. DAM; ISO 178
Flexural Modulus 330 MPa2mm / min. Conditioned; ISO 178
 530 MPa2mm / min. DAM; ISO 178
Charpy Impact, Notched 55.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1e/A
 95.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1e/A
 110 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1e/A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmConditioned. 500V; IEC 60093
 1.00e+13 ohm-cmDAM; 500V.; IEC 60093
Surface Resistance 1.00e+10 ohmConditioned. 500V; IEC 60093
 1.00e+12 ohmDAM; 500V.; IEC 60093
 
Thermal PropertiesOriginal ValueComments
Melting Point 217 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 100 °CISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °CISO 75/2Af
 
Processing PropertiesOriginal ValueComments
Processing Temperature 240 - 290 °CExtrusion Temperature
Melt Temperature 230 - 260 °CInjection Molding
Mold Temperature 70.0 - 80.0 °C
 
Descriptive Properties
Injection Molding Injection SpeedMedium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRADI6940 / 293445

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.