MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kolon KOPEL® KP3339UM Thermoplastic Polyester Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: TPC-ET. Injection Molding/Extrusion, PEL, General Purpose, Modest Modulus.

Flexibility and elastic recovery are similar to rubber, but the mechanical properties, heat resistance, weather resistance and UV stability are far better than the performance of conventional rubber.

Information provided by Kolon Plastic, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³ASTM D792
Water Absorption 0.70 %0.70 %ASTM D570
Linear Mold Shrinkage 0.0108 - 0.0112 cm/cm0.0108 - 0.0112 in/inASTM D955
Melt Flow 30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
30 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 3939ASTM D2240
Tensile Strength at Break 24.0 MPa3480 psi
Elongation at Break 1070 %
@Thickness 3.20 mm
1070 %
@Thickness 0.126 in
200 mm/min; ASTM D638
Flexural Strength 4.00 MPa
@Thickness 3.20 mm
580 psi
@Thickness 0.126 in
200 mm/min; ASTM D790
Flexural Modulus 0.0480 GPa6.96 ksi200 mm/min; ASTM D790
 
Thermal PropertiesMetricEnglishComments
Melting Point 195 °C383 °F20°C/min; ASTM D3418
Vicat Softening Point 138 °C
@Load 1.02 kg
280 °F
@Load 2.25 lb
ASTM D1525
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 180 - 190 °C356 - 374 °F
Middle Barrel Temperature 200 - 220 °C392 - 428 °F
Front Barrel Temperature 210 - 220 °C410 - 428 °F
Nozzle Temperature 210 - 220 °C410 - 428 °F
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °F
Drying Temperature 100 - 110 °C
@Time 10800 - 28800 sec
212 - 230 °F
@Time 3.00 - 8.00 hour
Dehumidifying Dryer
Moisture Content <= 0.10 %<= 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKOKZ754 / 255765

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.