MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
CHT CHT-BeauSil™ PEG 023 Silicone polymer
Categories: Other Engineering Material

Material Notes: Description: Organo modified Silicone polymer for the use as ingredient in Personal Care applications. The unique product allows to formulate high end formulations.

Key Features

  • Cleansing effect
  • Emulsifier for W/Si and W/O emulsions with dispersing and solubilizing properties
  • Enhances Spreading
  • Emollient and Conditioning agent
Key Applications
  • Hair Care
  • Skin Care
  • Color Cosmetic
  • Sun Care
Application: CHT-BeauSil™ PEG 023 is an emulsifier special for water – in – silicone emulsion as well as water – in – oil emulsion. The application fields for CHT-BeauSil™ PEG 023 are skin care and decorative cosmetic. CHT-BeauSil™ PEG 023 is suitable for making sun care products as well as body lotions.

Addition Rates
Dosage – 1: 0.5 - 3.0% as emulsifier

INCI Name: PEG-10 dimethicone

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles 0.00 %
Brookfield Viscosity 450 - 800 cP
Storage Temperature 4.00 - 40.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceColorless to yellow liquid
IonicityNon-ionic
MIT FreeYes
Ultralow cyclic contentYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHTSIL353 / 314836

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.