MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Alliance BCNU-201 Bonded Neo Ferrite Hybrid Magnet
Categories: Ceramic; Oxide; Metal; Electronic/Magnetic Alloy

Material Notes: Hybrid Bonded Magnets made by Compression Molding NdFeB and Ferrite powders with resins such as Nylon 6, Nylon 12 or PPS. The resulting grades have properties that cannot be achieved by typical Ferrite, SmCo or NdFeB sintered and bonded molding processes. Typical usage for a Hybrid magnet is a situation where the application requires more flux than can be provided by a Ferrite magnet but not to the level of a NdFeB magnet.

Information provided by Alliance LLC.

Key Words: Permanent Magnet
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 5.60 - 6.00 g/cc
 
Electrical PropertiesOriginal ValueComments
Magnetic Coercive Force, Hc 5000 - 5400 Oe
 9000 - 9500 OeIntrinsic
Magnetic Remanence, Br 6000 - 6400 Gauss
Magnetic Maximum Energy Product, BH 7.8 - 8.4 MGOe
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air <= 120 °CContinuous
 
Descriptive Properties
Reversible Temperature Coefficients-0.1Bd. %/°C
 -0.42Hd. %/°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NALLIAN9867 / 268421

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.