MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
China General Plastics Anti-Corrosion Liner
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: CGPC Anti-Corrosion Liner is a sheeting designed with "KEY" which is mechanically fixed to concrete pipe's or structure's internal surfaces during the manufacturing process to provide permanent protection against chemical attack.

Applications:

  • Pipe liner.
  • Manhole liner.
  • Treatment plant internal surface liner.
  • Substructures water-proofing and anti-corrosion.
  • Chemical plant storage compartments.

Information provided by China General Plastics Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption <= 0.10 %
@Time 86400 sec
sample size 76mm x 25mm by Thickness of sheet; ASTM D570
Solubility in Water <= 0.050 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 54 - 62
Tensile Strength >= 17.25 MPaboth longitudinal and Transverse to key; ASTM D412
Elongation at Break >= 225 %both longitudinal and Transverse to key; ASTM D412
Tear Strength >= 80.0 kN/mGrip Speed 8.5mm/s, both longitudinal and transverse to key; ASTM D1004
 
Descriptive Properties
Plasticiser Permanence<1.0%ASTM D1203-67 Method B, 24 hours at 90°C on 50Mm diam. disc

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCGPC084 / 255999

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.