MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

SABIC SILTEM™ Resin STM1700 Polyetherimide (PEI) (Europe)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: SILTEM™ STM1700 resin is a flexible polyetherimide(PEI)-siloxane copolymer designed for wire and cable applications. It offers a halogen free (according VDE 0472) flame retardant solution that also offers low smoke emission and toxicity. It is an amber colored transparent material that can be selfcolored and easily processed on conventional equipment. The material may also have a fit in flexible profiles or injection molded parts.

Features: Low Corrosivity,High Tensile Elongation,Flexible,Chemical Resistance,Low Smoke and Toxicity,High Heat Resistance,Good dimensional stability,Flame Retardant,Non-Halogenated

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Water Absorption at Saturation 0.76 %0.76 %ISO 62-1
Linear Mold Shrinkage, Flow 0.0087 - 0.0092 cm/cm
@Thickness 3.20 mm
0.0087 - 0.0092 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 7.0 g/10 min
@Load 6.60 kg,
Temperature 295 °C
7.0 g/10 min
@Load 14.6 lb,
Temperature 563 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080ASTM D2240
Tensile Strength at Break 59.0 MPa8560 psi50 mm/min; ISO 527
Tensile Strength, Yield 68.0 MPa9860 psi50 mm/min; ISO 527
Elongation at Break 15 %15 %50 mm/min; ISO 527
Elongation at Yield 5.0 %5.0 %50 mm/min; ISO 527
Tensile Modulus 2.30 GPa334 ksi1 mm/min; ISO 527
Flexural Strength 98.0 MPa14200 psiyield, 2 mm/min; ISO 178
Flexural Modulus 2.00 GPa290 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO) 16.0 kJ/m²7.61 ft-lb/in²80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Tear Strength 37.0 kN/m
@Thickness 1.60 mm
211 pli
@Thickness 0.0630 in
ISO 34 (Method A)
Taber Abrasion, mg/1000 Cycles 5050CS-17, 1 kg; ASTM D1044
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmASTM D257
Dielectric Constant  3.0
@Frequency 100000 Hz
3.0
@Frequency 100000 Hz
ASTM D150
 3.04
@Frequency 1e+6 Hz
3.04
@Frequency 1e+6 Hz
ASTM D150
 3.13
@Frequency 100 Hz
3.13
@Frequency 100 Hz
ASTM D150
Dielectric Strength 16.7 kV/mm
@Thickness 3.20 mm
424 kV/in
@Thickness 0.126 in
in oil; ASTM D149
Dissipation Factor  0.0054
@Frequency 1e+6 Hz
0.0054
@Frequency 1e+6 Hz
ASTM D150
 0.0061
@Frequency 100000 Hz
0.0061
@Frequency 100000 Hz
ASTM D150
 0.011
@Frequency 100 Hz
0.011
@Frequency 100 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Transformation Temperature, Tg 200 °C392 °FDMA
Deflection Temperature at 0.46 MPa (66 psi) 164 °C327 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
Vicat Softening Point 180 °C356 °FRate B/120; ISO 306
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
UL 94 by SABIC-IP
Oxygen Index 48 %48 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 320 - 330 °C608 - 626 °F
Zone 2 320 - 330 °C608 - 626 °F
Zone 3 320 - 330 °C608 - 626 °F
Melt Temperature 320 - 330 °C608 - 626 °FInjection Molding
Mold Temperature 110 - 120 °C230 - 248 °F
Drying Temperature 105 °C221 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 60 %40 - 60 %
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
Screw Speed 50 - 100 rpm50 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82488 / 290435

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.