MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Crosspolimeri GETILAN GPE/409 AFM Crosslinkable Polythene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: GETILAN: is the trade-mark of our crosslinkable polythene.

GETILAN GPE/409 AFM: chemically crosslinkable low smoke and low toxicity halogen free flame retardant compound for insulation and sheathing. It is a conveniently grafted polythene able to react in presence of moisture and of a catalyst. We normally suggest our catalyst type MAC/100 PSF. Where and when anti-ageing and anti-copper functions are required, we suggest our type MAC/203 or MAC/203 HSL (less in reaction). REACTION BETWEEN GRAFTING AND CATALYST These two compounds, separately stored, must be mixed before starting extrusion in the ratio: GRAFTING/CATALYST 97/3

Certify: CEI 2011 G10, VDE0207 2XI1

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/ccASTM D792
Melt Flow 0.50 - 3.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
Storage Temperature 12.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 14.0 MPaIEC 811
 15.12 MPa
@Temperature 135 °C,
Time 605000 sec
Heat Ageing; IEC 811
Elongation at Break 225 %IEC 811
 189 %
@Temperature 135 °C,
Time 605000 sec
Heat Ageing; IEC 811
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cmBS 6622
 
Thermal PropertiesOriginal ValueComments
Oxygen Index 25 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Zone 1 150 °C
Zone 2 160 °C
Zone 3 170 °C
Zone 4 180 °C
Die Temperature 205 °C
Head Temperature 195 °C
 
Descriptive Properties
Corrosivity of gases evolved> 4,3 pHIEC 754-2
Halogen Content0IEC 754-1
Hot Set Test0Residual Value, IEC 60811
 0.3200°C - 20 N/cm2, IEC 60811
Water absorption0.8 mg/cm²24 h at 100°C, IEC 811

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCROS119 / 294203

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.