MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Go Yen Chemical GoyenchemAO-1330 Antioxidant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: CAS No. 1709-70-2

Applications:

  • polyolefins : polyethylene, polypropylene, polybutene for the stabilization of pipes, molded articles, wires and cables, dielectric films etc.
  • polymers :engineering plastics like linear polyesters, polyamides, styrene homo and copolymers.
  • PVC, polyurethanes, elastomers, adhesives, and other organic substrates.

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.480 - 0.570 g/ccGF
 0.530 - 0.630 g/ccPowder
Density 1.04 g/cc
Volatiles <= 0.10 %
Molecular Weight 775 g/mol
Ash <= 0.10 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 240 - 245 °C
Boiling Point >= 200 °C
Flash Point 321 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible >= 98 %
@Wavelength 425 nm
 >= 99 %
@Wavelength 500 nm
 
Descriptive Properties
AppearanceWhite, free-flowing powder
Assay>98%
Solubility<0.1 g/100g solutionWater
 10 g/100g solutionn-Hexane
 18 g/100g solutionAcetone
 27 g/100g solutionEthylacetate
 28 g/100g solutionChloroform
 3 g/100g solutionMethanol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN526 / 266834

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.