MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Radici Radilon® DT 40E50USR 333C BK Polyamide 612
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Unreinforced

Material Notes: PA612 semi-rigid, high viscosity extrusion grade. Toughened. Improved resistance to uric acid solutions. Black color.

Suitable for extrusion of profiles, tubes, and pipes. Material especially developed for automotive under the hood applications, employed in selective catalytic reductions systems (SCR).

Information provided by Radici Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³DAM; ISO 1183
Water Absorption 2.0 %
@Thickness 2.00 mm,
Time 86400 sec
2.0 %
@Thickness 0.0787 in,
Time 24.0 hour
Immersion @ 23°C; ISO 62
Moisture Absorption 0.800 %
@Thickness 2.00 mm,
Temperature 23.0 °C
0.800 %
@Thickness 0.0787 in,
Temperature 73.4 °F
50% RH; ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 31.0 MPa4500 psi50mm/min. DAM; ISO 527-2/1A
Tensile Modulus 0.950 GPa138 ksi1mm / min. DAM; ISO 527-2/1A
Flexural Strength 30.0 MPa4350 psi2mm / min. DAM; ISO 178
Flexural Modulus 0.750 GPa109 ksi2mm / min. DAM; ISO 178
Charpy Impact, Notched  6.80 J/cm²
@Temperature -30.0 °C
32.4 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1e/A
 7.50 J/cm²
@Temperature -30.0 °C
35.7 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1e/A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmConditioned. 500V; IEC 60093
 1.00e+13 ohm-cm1.00e+13 ohm-cmDAM; 500V.; IEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 212 °C414 °F10°C/min; ISO 11357-1/-3
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 220 °C428 °F
 250 °C482 °F
Front Barrel Temperature 260 °C500 °F
 270 °C518 °F
Die Temperature 275 - 280 °C527 - 536 °F
Melt Temperature 275 °C527 °F
Head Temperature 275 - 280 °C527 - 536 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRADI6946 / 293451

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.