MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Primex Plastics Prime HMWPE 1000 Swirl High Molecular Weight Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Prime HMWPE 1000 Swirl material consists of a HMWPE substrate with a three-color swirl cap of HMWPE. The swirl can be on one or both sides of the sheet. The thickness can be varied to suit your specific material requirements and draw ratios.

Applications: Applications so far have consisted of playground equipment, camouflage deer blinds, canoes, and other sporting equipment.

Information provided by Primex Plastics Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.949 g/cc0.949 g/ccASTM D1505
Environmental Stress Crack Resistance >= 600 hour>= 600 hourASTM D1693
Melt Flow 10 g/10 min10 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 24.8 MPa3600 psiASTM D638
Elongation, Ultimate >= 600 %>= 600 %ASTM D638
Flexural Modulus 1.17 GPa170 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 124 °C256 °FASTM D1525
Flammability, UL94 HB
@Thickness >=1.52 mm
HB
@Thickness >=0.0600 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPRIM020 / 278491

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.