MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ ELCRIN™ 61000PUiQ2 Polycarbonate + PBT (PC+PBT)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Material Notes: LNP ELCRIN 61000PUiQ2 (also known as ELCRIN ER011364) is based on Polycarbonate / Polybutylene Terephthalate (PC/PBT) alloy, utilizing iQ PBT generation 2 technology with 23% post consumer recycled content. Added features of this material include: excellent low temperature impact strength, improve retention of mechanical properties under UV exposure, good surface aesthetics, good chemical resistance and easy flow ability.

Features: Sustainability,Post-Consumer Recycled (PCR) content,Aesthetics and Appearance,Enhanced Low Temperature Impact,Chemical Resistance,UV Resistant,High Impact Resistance,High Flow

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.24 g/cc1.24 g/ccASTM D792
Density 1.24 g/cc0.0448 lb/in³ISO 1183
Water Absorption 0.12 %
@Time 86400 sec
0.12 %
@Time 24.0 hour
ISO 62-1
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.0700 %0.0700 %23°C/50% RH/24 hrs; ISO 62-4
Viscosity 42 cP
@Load 5.00 kg,
Temperature 250 °C
42 cP
@Load 11.0 lb,
Temperature 482 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0090 cm/cm0.0090 in/inSABIC method
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/inSABIC method
Melt Flow 46 g/10 min
@Load 5.00 kg,
Temperature 250 °C
46 g/10 min
@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 40.0 MPa5800 psi50 mm/min; ASTM D638
 45.0 MPa6530 psi50 mm/min; ISO 527
Tensile Strength, Yield 50.0 MPa7250 psi50 mm/min; ASTM D638
 52.0 MPa7540 psi50 mm/min; ISO 527
Elongation at Break 115 %115 %50 mm/min; ASTM D638
 159 %159 %50 mm/min; ISO 527
Elongation at Yield 5.0 %5.0 %50 mm/min; ASTM D638
 5.0 %5.0 %50 mm/min; ISO 527
Tensile Modulus 2.02 GPa293 ksi50 mm/min; ASTM D638
 2.04 GPa296 ksi1 mm/min; ISO 527
Flexural Strength 78.0 MPa11300 psiyield, 2 mm/min; ISO 178
 80.0 MPa11600 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.07 GPa300 ksi1.3 mm/min, 50 mm span; ASTM D790
 2.125 GPa308.2 ksi2 mm/min; ISO 178
Izod Impact Notched 560 J413 ft-lbASTM D256
 240 J
@Temperature -40.0 °C
177 ft-lb
@Temperature -40.0 °F
ASTM D256
 530 J
@Temperature 0.000 °C
391 ft-lb
@Temperature 32.0 °F
ASTM D256
Izod Impact, Notched (ISO) 41.0 kJ/m²19.5 ft-lb/in²80*10*4; ISO 180/1A
 17.0 kJ/m²
@Temperature -40.0 °C
8.09 ft-lb/in²
@Temperature -40.0 °F
80*10*4; ISO 180/1A
 40.0 kJ/m²
@Temperature 0.000 °C
19.0 ft-lb/in²
@Temperature 32.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 4.30 J/cm²20.5 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 1.60 J/cm²
@Temperature -40.0 °C
7.61 ft-lb/in²
@Temperature -40.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 4.00 J/cm²
@Temperature 0.000 °C
19.0 ft-lb/in²
@Temperature 32.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 49.0 J36.1 ft-lbpeak; ASTM D3763
 54.0 J39.8 ft-lbASTM D3763
Dart Drop Test 510000 g1120 lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 120 - 180 sec120 - 180 secASTM D495
Comparative Tracking Index 400 - 600 V400 - 600 VUL 746A
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness >=1.50 mm
15 - 30 sec
@Thickness >=0.0591 in
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness >=1.50 mm
>= 120 arcs
@Thickness >=0.0591 in
UL 746A
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min0.000 - 0.394 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 86.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
47.8 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow 88.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
48.9 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °C208 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 101 °C
@Thickness 3.20 mm
214 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 73.0 °C163 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 80.0 °C
@Thickness 3.20 mm
176 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 113 °C235 °FRate B/50; ASTM D1525
 117 °C243 °FRate B/120; ASTM D1525
UL RTI, Electrical 75.0 °C167 °FUL 746B
UL RTI, Mechanical with Impact 75.0 °C167 °FUL 746B
UL RTI, Mechanical without Impact 75.0 °C167 °FUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
HB
@Thickness >=0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 235 - 265 °C455 - 509 °F
Zone 2 235 - 265 °C455 - 509 °F
Zone 3 235 - 265 °C455 - 509 °F
Melt Temperature 235 - 265 °C455 - 509 °FInjection Molding
Mold Temperature 40.0 - 65.0 °C104 - 149 °F
Drying Temperature 110 °C230 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 50 - 80 %50 - 80 %
Vent Depth 0.00130 - 0.00200 cm0.000512 - 0.000787 in
Screw Speed 50 - 80 rpm50 - 80 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF2UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80605 / 288552

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.