MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ExOne Inconel 718 for 3D Printing
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Nonferrous Metal; Nickel Alloy

Material Notes:

Information provided by ExOne™

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.13 g/cc0.294 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 41.041.0
Tensile Strength, Ultimate 1310 MPa190000 psiX & Y
 1331 MPa193000 psiZ
Tensile Strength, Yield 1069 MPa155000 psiX & Y
 1076 MPa156100 psiZ
Elongation at Break 15.0 %15.0 %X & Y
 15.0 %15.0 %Z
Modulus of Elasticity 193 GPa28000 ksiX & Y
 193 GPa28000 ksiZ
Poissons Ratio 0.2900.290
Impact Test 12.2 J9.00 ft-lb
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.200 - 0.800 %0.200 - 0.800 %
Boron, B <= 0.00600 %<= 0.00600 %
Carbon, C 0.0400 - 0.130 %0.0400 - 0.130 %
Chromium, Cr 17.0 - 21.0 %17.0 - 21.0 %
Cobalt, Co <= 1.00 %<= 1.00 %
Copper, Cu <= 0.300 %<= 0.300 %
Iron, Fe 11.1 - 24.6 %11.1 - 24.6 %balance
Manganese, Mn <= 0.350 %<= 0.350 %
Molybdenum, Mo 2.80 - 3.30 %2.80 - 3.30 %
Nb + Ta 4.75 - 5.50 %4.75 - 5.50 %
Nickel, Ni 50.0 - 55.0 %50.0 - 55.0 %
Phosphorus, P <= 0.0150 %<= 0.0150 %
Silicon, Si <= 0.350 %<= 0.350 %
Sulfur, S <= 0.0150 %<= 0.0150 %
Titanium, Ti 0.650 - 1.15 %0.650 - 1.15 %
 
Descriptive Properties
Surface Roughness3.6 µm Ra

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NEXONE994 / 323299

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.