MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Pressure Seal 9819 Fluorinated Hydrocarbon
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 9819 is an 80 durometer black colored Fluorinated Hydrocarbonelastomer, it is formulated with Graphite to provide internal lubrication. It exhibits excellent resistance to heat, compression set, petroleum based oils, aliphatic and aromatic fuels.

This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 HK 810 A1-10 B37 B38 EO78; 4 HK 810 A1-11 B38 EO78; 6 HK 810 A1-10 A1-11 B31 B38 EO88

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.87 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 79
 71
@Temperature 200 °C,
Time 252000 sec
Stauffer Blend 7700
 73
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel C
 75
@Temperature 200 °C,
Time 252000 sec
Service Fluid 101
 76
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel B
 77
@Temperature 100 °C,
Time 252000 sec
Distilled water aged
 78
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #1
 78
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #3
 79
@Temperature 250 °C,
Time 252000 sec
Heat Aged
 81
@Temperature 275 °C,
Time 252000 sec
Heat Aged
Tensile Strength 1440 psi
 1183.7 psi
@Temperature 200 °C,
Time 252000 sec
Service Fluid 101
 1255.7 psi
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel C
 1261.4 psi
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel B
 1368 psi
@Temperature 100 °C,
Time 252000 sec
Distilled water aged
 1429.9 psi
@Temperature 275 °C,
Time 252000 sec
Heat Aged
 1458.7 psi
@Temperature 250 °C,
Time 252000 sec
Heat Aged
 1460.2 psi
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #3
 1566.7 psi
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #1
 1746.7 psi
@Temperature 200 °C,
Time 252000 sec
Stauffer Blend 7700
Elongation, Ultimate 175 %
 154 %
@Temperature 250 °C,
Time 252000 sec
Heat Aged
 154 %
@Temperature 200 °C,
Time 252000 sec
Service Fluid 101
 159.1 %
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel C
 166.9 %
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel B
 175 %
@Temperature 200 °C,
Time 252000 sec
Stauffer Blend 7700
 175 %
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #1
 183.9 %
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #3
 187.1 %
@Temperature 275 °C,
Time 252000 sec
Heat Aged
 204.1 %
@Temperature 100 °C,
Time 252000 sec
Distilled water aged
100% Modulus 1015 psi
Tear Strength 176 pliDie B
Compression Set 7.5 %
@Temperature 23.0 °C,
Time 79200 sec
Solid
 8.3 %
@Temperature 175 °C,
Time 79200 sec
Solid
 9.6 %
@Temperature 23.0 °C,
Time 79200 sec
Plied
 10.1 %
@Temperature 200 °C,
Time 79200 sec
Solid
 11.1 %
@Temperature 175 °C,
Time 79200 sec
Plied
 11.9 %
@Temperature 200 °C,
Time 79200 sec
Plied
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature 0.000 °F
Shrinkage -1.80 %
@Temperature 275 °C,
Time 252000 sec
Weight, Heat Aged
 -1.00 %
@Temperature 250 °C,
Time 252000 sec
Weight, Heat Aged
 0.20 %
@Temperature 150 °C,
Time 252000 sec
Volume, ASTM Oil #1
 1.3 %
@Temperature 150 °C,
Time 252000 sec
Volume, ASTM Oil #3
 1.3 %
@Temperature 23.0 °C,
Time 252000 sec
Volume, ASTM Reference Fuel B
 2.6 %
@Temperature 23.0 °C,
Time 252000 sec
Volume, ASTM Reference Fuel A
 3.1 %
@Temperature 23.0 °C,
Time 252000 sec
Volume, ASTM Reference Fuel C
 9.1 %
@Temperature 200 °C,
Time 252000 sec
Volume, Service Fluid 100
 17.6 %
@Temperature 200 °C,
Time 252000 sec
Volume, Stauffer Blend 7700
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRESL129 / 318339

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.