Temper: Extra Hard Fabrication Properties: Excellent Suitability – Soldering, Brazing, Gas Shielded Arc Welding, Capacity for Being Cold Worked; Good Suitability – Oxyacetylene Welding, Butt Weld; Fair Suitability – Capacity for Being Hot Formed Typical Uses: Terminals, automotive; Connectors, electronic; Contact springs; Lead Frames Applicable Specifications: Bar – ASTM B591; Strip – ASTM B888/B88M, ASTM B591 |