MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Nouryon DIBAL-H Diisobutylaluminum hydride, Polymer
Categories: Other Engineering Material

Material Notes: DIBAL-H is a co-catalyst product soluble in aromatic and saturated aliphatic and cycloaliphatic hydrocarbons.

CAS number: 1191-15-7

EINECS/ELINCS No.: 214-729-9

Applications: DIBAL-H is used as a cocatalyst in the Ziegler-Natta polymerization of olefins and as a reducing agent in organic synthesis.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.797 g/cc0.0288 lb/in³
Viscosity 13.5 cP
@Temperature 30.0 °C
13.5 cP
@Temperature 86.0 °F
Molecular Weight 142.2 g/mol142.2 g/mol
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 297 J/g128 BTU/lb?Hv, NBP / 1 bar
Specific Heat Capacity 2.146 J/g-°C
@Temperature 57.0 °C
0.5129 BTU/lb-°F
@Temperature 135 °F
Melting Point -80.0 °C-112 °F
Boiling Point 114 °C
@Pressure 0.0001333 MPa
237 °F
@Pressure 0.01933 psi
Heat of Formation -402 kJ/mol-402 kJ/mol?Hf°, 25 °C / 1 bar
 
Descriptive Properties
AppearanceClear, colorless liquid
Content= 3.0 wt%Triisobutylaluminum
 = 97.0 wt%Diisobutylaluminum hydride
 18.8 wt%Aluminum
Heat of combustion-6410 kJ/moleΔHc°, 25 °C
Heat of hydrolysis3523 J/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY480 / 286003

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.