MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Angst+Pfister APSOplast® PA 6 G SL PA 6 cast polyamide + solid lubricant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: This special cast polyamide PA 6 G has an evenly distributed, embedded solid lubricant which gives this self lubricating material excellent sliding properties, exceptional wear resistance, and an extraordinary dynamic load-bearing capacity (a PV limit value of up to 5 times higher than traditional cast polyamide types). This material is particularly suited to high sliding speeds in the case of non-lubricated bearings and wearing parts and is thus the perfect complement to oil-filled PA 6 G LO.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccDIN EN ISO 1183-1
Moisture Absorption 2.00 %at saturation in standardized climate; DIN EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 81DIN EN ISO 868
Ball Indentation Hardness 170 MPaDIN EN ISO 2039-1
Tensile Strength, Yield 75.0 MPa50 mm/min; DIN EN ISO 527
Elongation at Break >= 35 %50 mm/min; DIN EN ISO 527
Modulus of Elasticity 3.40 GPa1 mm/min; DIN EN ISO 527
Charpy Impact, Notched >= 3.50 kJ/m²DIN EN ISO 179-1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
DIN 53752
Specific Heat Capacity 1.70 J/g-°C
Thermal Conductivity 0.250 W/m-K
Melting Point 215 °CISO 11357-3
Maximum Service Temperature, Air 110 °Cshort term
 160 °Clong term
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °CDIN EN ISO 75/A
Minimum Service Temperature, Air -40.0 °C
Flammability, UL94 HB
@Thickness 3.00 mm
 HB
@Thickness 6.00 mm
 
Descriptive Properties
Colorgrey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PANGP036 / 250534

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.