OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approx. 500 g/mol (HMW-PE) Properties: UV stabilized; EU 1935/2004 & 10/2011 – conform; FDA – conform Color: UV – black FN9100/similar RAL9005 Range of applications: Mechanical engineering; Conveying industry; Outdoor applications Information provided by Okulen |