System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Nouryon Berol 185 PO
Categories:
Other Engineering Material
Material Notes:
EU Ecolabel-compliant version of Berol 185 using certified RSPO MB raw materials. It is a non-ionic surfactant, is hydrophilic, with excellent wetting, emulsifying and degreasing properties.
Information provided by Nouryon
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.02
g/cc
pH
5.0 - 7.0
1% in water
Viscosity
100
cP
Surface Tension
30
dynes/cm
according to Du Noüy, 25°C, 0.1%; DIN 53914
Thermal Properties
Original Value
Comments
Flash Point
>=
100
°C
Component Elements Properties
Original Value
Comments
H2O, Water
10 %
Descriptive Properties
Appearance
Clear liquid
Clear point
5 °C
Cloud point
64-70°C
1% in water
Color
= 100 Hazen
Content(%)
0
Primary + Secondary Amine
90
Active content
Foam Height according to Ross-Miles
110 mm
immediately, 50°C, 0.05%
20 mm
after 5 min, 50°C, 0.05%
HLB
13.5
Wetting power
10 sec
according to Draves, 25°C, 0.1%
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PNOURY377 / 285900
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.