MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chemours Teflon™ Type CLZ, one side cementable ETFE film
Categories: Polymer; Film; Thermoplastic

Material Notes: Tefzel™ ETFE film is a transparent, thermoplastic film that can be heat sealed, thermoformed, vacuum formed, heat bonded, welded, metallized, laminated (combined with dozens of other materials), and used as an excellent hot melt adhesive. This wide variety of fabrication possibilities combines with the following important properties to offer a unique balance of capabilities not available in other plastic films. Features: Chemical Compatibility, Electrical Reliability, Wide Thermal Range, Mechanical Toughness, Long Time Weather ability, Reliability.

Information provided by Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.70 g/ccASTM D1505
Water Absorption <= 0.030 %
@Time 86400 sec
ASTM D570
Moisture Absorption <= 0.0200 %
Specific Surface Area 4.0 m²/g
 10 m²/g
 20 m²/g
Water Vapor Transmission 0.500 g/100 in²/dayASTM E96
Oxygen Transmission 1600 cc-mm/m²-24hr-atmASTM D1434
Nitrogen Transmission 500 cc-mm/m²-24hr-atmASTM D1434
Carbon Dioxide Transmission 3900 cc-mm/m²-24hr-atmASTM D1434
Thickness 1.00 mil
 2.00 mil
 5.00 mil
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 72ASTM D2240
Tensile Strength at Break 6000 psiASTM D882
Tensile Strength 43.0 MPaASTM D1457
Elongation at Break 300 %ASTM D882
Flexural Modulus 0.830 GPaASTM D882
Flex Crack Resistance 50000Cycles MIT Folding Endurance; ASTM D2176
Izod Impact, Notched NBASTM D256
Coefficient of Friction, Dynamic 0.20 - 0.30Film-to-Steel; ASTM D1894
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+17 ohm-cmASTM D257
Surface Resistivity per Square >= 1.00e+15 ohmASTM D257
Dielectric Constant 2.6
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 160 kV/mm
@Thickness 0.0250 mm
Short-time, in air; ASTM D149 Method A
Dissipation Factor 0.00070ASTM D150
Arc Resistance 122 secASTM D495
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.280 BTU/lb-°F
Thermal Conductivity 0.240 W/m-KCenco-Fitch
Melting Point 260 - 280 °CASTM D3418
Flammability, UL94 V-0
Oxygen Index 30 %
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.40ASTM D542
Transmission, Visible 90 %Solar Transmission; ASTM E-424
 
Descriptive Properties
Chemical/Solvent ResistanceExcellentASTM D543
Dimensional Stability1% shrinkage.MD. 30 minutes at 150°C
 5% shrinkage.TD. 30 minutes at 150°C
Heat of Combustion13.7 MJ/kgASTM D240
Salt Spray Resistance Coatings (hours)1000ASTM B117. 5% NaCl at 35 °C (95 °F).
Tear Strength-Initial (Graves)500 gASTM D1004
Tear Strength-Propagating (Elmendorf)75 gASTM D 1922
Weather Resistance (years unaffected)15Florida Exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDU8850 / 268777

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.