MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Epoxies, Etc 50-2151 FR Polyurethane Thermally Conductive Potting & Encapsulating Compound
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Description: 50-2151 FR is a high performance thermally conductive two component urethane system. This easy to use polyurethane is low in viscosity and ideal for potting or encapsulating delicate electronic components. 50-2151 FR exhibits very low shrinkage, stress, and exotherm throughout the cure cycle. This system is also well known for its outstanding thermal shock and excellent dielectric properties. 50-2151 FR is formulated to be flame retardant. It is a good choice when heat transfer and electrical insulation properties are required.

Features:

  • Does not contain MOCA or TDI
  • Low viscosity
  • Very good thermal shock and vibration resistance
Benefits:
  • Low stress on components
  • Easy to handle
  • Low shrinkage

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.23 g/cc1.23 g/ccIsocyanate
 1.66 g/cc1.66 g/ccPolyol
Viscosity 200 cP200 cPIsocyanate
 10000 cP10000 cPMixed
 30000 cP30000 cPPolyol
Storage Temperature 18.0 - 27.0 °C64.4 - 80.6 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D  40
@Temperature 100 °C
40
@Temperature 212 °F
 50
@Temperature 25.0 °C
50
@Temperature 77.0 °F
 50
@Temperature 60.0 °C
50
@Temperature 140 °F
Tensile Strength 7.067 MPa1025 psi
Elongation at Break 30 %30 %
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 6.80e+13 ohm-cm6.80e+13 ohm-cm
Surface Resistance 1.80e+17 ohm1.80e+17 ohm
Dielectric Constant 4.0
@Frequency 100 Hz
4.0
@Frequency 100 Hz
Dielectric Strength 21.3 kV/mm540 kV/in
Dissipation Factor 0.18
@Frequency 100 Hz
0.18
@Frequency 100 Hz
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.15 W/m-K7.98 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 130 °C266 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Shrinkage <= 1.0 %<= 1.0 %
 
Processing PropertiesMetricEnglishComments
Cure Time  40.0 min
@Temperature 85.0 °C
0.667 hour
@Temperature 185 °F
 90.0 min
@Temperature 65.0 °C
1.50 hour
@Temperature 149 °F
 150 min
@Temperature 45.0 °C
2.50 hour
@Temperature 113 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 70.0 min
@Load 0.100 kg
70.0 min
@Load 0.221 lb
 
Descriptive Properties
ColorTan
Mix Ratio100:12By weight (Polyol, Isocyanate)
 100:16By volume (Polyol, Isocyanate)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFEPOX044 / 316721

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.