40% glass fiber, enhanced strength and stress crack resistant, natural color Ryton® R-4-240NA and R-4-240BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and toughness compared to other polyphenylene sulfide compounds. Markets/Uses: Automotive / Fuel Systems / Sender Units Applications: Automotive Applications Features: Good Strength; Good Toughness Information provided by Solvay Specialty Polymers. |