MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Abhar Polymer Compounds APPEX15 Silane cross-linkable PE compound
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: APPEX15 is a pre-grafted polyethylene which can be processed in combination with its catalyst master batch (APCAT12N) in conventional extruders. Cross linking happen by exposing end products to moisture. It's used for domestic hot and cold water, under floor heating and central heating.

Information provided by Abhar Polymer Compounds

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 - 0.950 g/ccASTM D792
Melt Flow 0.70 - 0.90 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ASTM D1238
Storage Temperature <= 35.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 25.0 MPaASTM D638
Elongation at Break >= 600 %ASTM D638
 
Processing PropertiesOriginal ValueComments
Zone 1 160 - 170 °C
Zone 2 170 - 180 °C
Zone 3 180 - 190 °C
Zone 4 180 - 190 °C
Die Temperature 210 - 220 °C
Head Temperature 200 - 210 °C
Drying Temperature 60.0 °C
@Time 7200 sec
Moisture Content <= 0.020 %
@Temperature 80.0 °C,
Time 7200 sec
QCW01
Shelf Life 6.00 Month
 
Descriptive Properties
ColorNatural
Gel content>65%STM D2765

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PABHAR013 / 249446

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.