MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ ELCRES™ EXL7414 Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP ELCRES EXL7414 is based on Polycarbonate (PC) siloxane copolymer resin. It is a medium flow, non-chlorinated, non-brominated flame retardant opaque grade. It offers excellent low temperature ductility (-40C), extremely thin wall flame retardant capability with UL94 V0 at 0.6mm, and in combination with excellent processability and release with opportunities for shorter cycle times compared to standard Polycarbonate. It is available in wide range of opaque colors and is an excellent candidate for a wide variety of applications such as the battery cover of fast-charging mobile phones that need to be compliant with IEC62368-1.

Features: Enhanced Low Temperature Impact,Flame Retardant,Non-Chlorinated,Non-Brominated,High Impact Resistance,Good Mold Release,Exceptional Processing

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Viscosity 11 cP
@Load 1.20 kg,
Temperature 300 °C
11 cP
@Load 2.65 lb,
Temperature 572 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0040 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0080 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0080 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 12 g/10 min
@Load 1.20 kg,
Temperature 300 °C
12 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 8484ASTM D785
Hardness, Rockwell R 117117ASTM D785
Tensile Strength at Break 61.0 MPa8850 psi50 mm/min; ASTM D638
 61.0 MPa8850 psi50 mm/min; ISO 527
Tensile Strength, Yield 53.0 MPa7690 psi50 mm/min; ASTM D638
 54.0 MPa7830 psi50 mm/min; ISO 527
Elongation at Break 120 %120 %50 mm/min; ASTM D638
 120 %120 %50 mm/min; ISO 527
Elongation at Yield 5.2 %5.2 %50 mm/min; ISO 527
 5.3 %5.3 %50 mm/min; ASTM D638
Tensile Modulus 2.12 GPa307 ksi50 mm/min; ASTM D638
 2.15 GPa312 ksi1 mm/min; ISO 527
Flexural Strength 84.0 MPa12200 psiyield, 2 mm/min; ISO 178
 88.0 MPa12800 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.13 GPa309 ksi2 mm/min; ISO 178
 2.15 GPa312 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 900 J664 ft-lbASTM D256
 700 J
@Temperature -40.0 °C
516 ft-lb
@Temperature -40.0 °F
ASTM D256
 770 J
@Temperature -30.0 °C
568 ft-lb
@Temperature -22.0 °F
ASTM D256
 850 J
@Temperature 0.000 °C
627 ft-lb
@Temperature 32.0 °F
ASTM D256
Izod Impact, Notched (ISO) 73.0 kJ/m²34.7 ft-lb/in²80*10*3; ISO 180/1A
 65.0 kJ/m²
@Temperature -30.0 °C
30.9 ft-lb/in²
@Temperature -22.0 °F
80*10*3; ISO 180/1A
Charpy Impact, Notched 7.80 J/cm²37.1 ft-lb/in²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 6.90 J/cm²
@Temperature -30.0 °C
32.8 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 69.0 J50.9 ft-lbASTM D3763
 66.0 J
@Temperature -30.0 °C
48.7 ft-lb
@Temperature -22.0 °F
ASTM D3763
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmASTM D257
Surface Resistance >= 1.00e+16 ohm>= 1.00e+16 ohmASTM D257
Dielectric Constant  2.81
@Frequency 1.90e+9 Hz
2.81
@Frequency 1.90e+9 Hz
SABIC method
 2.81
@Frequency 5.00e+9 Hz
2.81
@Frequency 5.00e+9 Hz
SABIC method
 2.84
@Frequency 1e+10 Hz
2.84
@Frequency 1e+10 Hz
SABIC method
 2.87
@Frequency 1.10e+9 Hz
2.87
@Frequency 1.10e+9 Hz
SABIC method
Dissipation Factor  0.0060
@Frequency 1.90e+9 Hz
0.0060
@Frequency 1.90e+9 Hz
SABIC method
 0.0060
@Frequency 5.00e+9 Hz
0.0060
@Frequency 5.00e+9 Hz
SABIC method
 0.0061
@Frequency 1e+10 Hz
0.0061
@Frequency 1e+10 Hz
SABIC method
 0.0064
@Frequency 1.10e+9 Hz
0.0064
@Frequency 1.10e+9 Hz
SABIC method
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  77.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
42.8 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 88.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
48.9 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow  87.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
48.3 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 98.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
54.4 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 119 °C246 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 118 °C
@Thickness 3.20 mm
244 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 108 °C226 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 105 °C
@Thickness 3.20 mm
221 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 123 °C253 °FRate B/50; ISO 306
 124 °C255 °FRate B/120; ISO 306
UL RTI, Electrical 80.0 °C176 °FUL 746B
UL RTI, Mechanical with Impact 80.0 °C176 °FUL 746B
UL RTI, Mechanical without Impact 80.0 °C176 °FUL 746B
Flammability, UL94  V-0
@Thickness >=0.600 mm
V-0
@Thickness >=0.0236 in
UL 94
 5VB
@Thickness >=3.00 mm
5VB
@Thickness >=0.118 in
UL 94
Oxygen Index 38 %38 %ISO 4589
Glow Wire Ignition Temperature 850 °C
@Thickness 1.00 mm
1560 °F
@Thickness 0.0394 in
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 290 - 310 °C554 - 590 °F
Zone 2 280 - 305 °C536 - 581 °F
Zone 3 295 - 315 °C563 - 599 °F
Melt Temperature 295 - 315 °C563 - 599 °FInjection Molding
Mold Temperature 70.0 - 95.0 °C158 - 203 °F
Drying Temperature 110 °C230 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 48.0 hour48.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 60 %40 - 60 %
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80592 / 288539

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.