MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Corr-Paint™ CP4000-S2 High Temperature Protective Coating Silicone
Categories: Other Engineering Material; Ceramic/Metallic Coating; Polymer; Thermoset; Silicone

Material Notes: Aremco’s Corr-Paint™ CP40xx-S2 series silicone-ceramic coatings are single-part, room temperature cure systems that provide ultra-high temperature resistance up to 1800 oF (982 oC) along with exceptional resistance to outdoor weathering, UV, salt-spray corrosion, and flame impingement.

Product Highlights

  • Ultra-High Temperature Resistance
  • Room Temperature Curing
  • Single Part, No Catalyst Required
  • Sprayable, Low Viscosity
  • Moisture & Salt Spray Resistant
  • Flame Resistant
  • UV Resistant
  • High Dielectric Strength
Typical Applications
  • Ultra-High Temperature Resistance
  • Room Temperature Curing
  • Single Part, No Catalyst Required
  • Sprayable, Low Viscosity
  • Moisture & Salt Spray Resistant
  • Flame Resistant
  • UV Resistant
  • High Dielectric Strengthers

Key Words: High Temperature Coatings
Vendors: Aremco’s Corr-Paint™ CP40xx-S2 series silicone-ceramic coatings are single-part, room temperature cure systems that provide ultra-high temperature resistance. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.43 g/cc1.43 g/cc
Solids Content 77.1 %77.1 %by volume
 83 %83 %by weight
Volatile Organic Compounds (VOC) Content 217 g/l217 g/l
Viscosity 250 - 500 cP250 - 500 cPBrookfield LV Viscometer
Thickness 25.4 microns1.00 milrecommended dry film thickness
 33.8 microns1.33 milestimated wet film thickness
Storage Temperature 4.44 - 32.2 °C40.0 - 90.0 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 538 °C1000 °FContinuous
 1200 °C2190 °FIntermittent
Flash Point 47.8 °C118 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 10.0 - 48.9 °C50.0 - 120 °FApplication Temperature
Dry Time 1.00 - 2.00 hour1.00 - 2.00 hourTouch
 2.00 - 4.00 hour2.00 - 4.00 hourHandling
 1.00 - 24.0 hour1.00 - 24.0 hourRecoat
Cure Time 1440 - 2880 min24.0 - 48.0 hourRT
 60.0 min
@Temperature 232 °C
1.00 hour
@Temperature 450 °F
1 hr minimum Air set
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
ColorBlack
Dry Film Coverage ft2/gal1236at 1 mil
Thinnert-Butyl Acetate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAREM75am / 282879

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.