System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Lanxess Pocan® KU 1-7635 POS151 000000 PBT + PC, 30% Glass Fiber
(Unverified Data**)
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
;
Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
Material Notes:
PBT+PC, 30% glass fibers, injection molding, low tendency to warp, improved surface finish, UV-stabilized
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.50
g/cc
ISO 1183
Water Absorption
0.30 %
Test Sim. to ISO 62
Moisture Absorption at Equilibrium
0.10 %
23°C/50% R.H.; Test Sim. to ISO 62
Linear Mold Shrinkage, Flow
0.0035
cm/cm
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse
0.0045
cm/cm
ISO 294-4, 2577
Melt Flow
21
g/10 min
@Load 2.16 kg,
Temperature 260 °C
Estimated using room temperature density; ISO 1133
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
100
MPa
ISO 527-1/-2
Elongation at Break
2.5 %
ISO 527-1/-2
Tensile Modulus
7500
MPa
ISO 527-1/-2
Charpy Impact Unnotched
50.0
kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Electrical Properties
Original Value
Comments
Comparative Tracking Index
150
V
IEC 60112
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
30.0
µm/m-°C
ISO 11359-1/-2
CTE, linear, Transverse to Flow
80.0
µm/m-°C
ISO 11359-1/-2
Melting Point
225
°C
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi)
165
°C
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi)
120
°C
ISO 75-1/-2
Flammability, UL94
HB
@Thickness 0.800 mm
IEC 60695-11-10
HB
@Thickness 1.60 mm
IEC 60695-11-10
Processing Properties
Original Value
Comments
Melt Temperature
260
°C
Injection Molding; ISO 294
Mold Temperature
80.0
°C
Injection Molding; ISO 10724
Descriptive Properties
Additives
Release agent
Features
U.V. stabilized or stable to weather
Form
Pellets
ISO Short Name
ISO 7792-1-PBT+PC,GHLMR,09-080,GF30
Processing
Injection molding
Region
Asia Pacific
Europe
Near East/Africa
North America
South and Central America
**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Envalior Pocan® A 3131 000000 PBT+PC, 30% Glass Fiber Reinforced
Mitsubishi Novaduran® 5010G30 Polybutylene Terephthalate
LG Chemical Lupox® PBT-GP-2306FA 30% GFR Flame Retardant, UV Stabilized PBT
Envalior Pocan® C 3230 XF 000000 PBT+PC, 30% Glass Fiber Reinforced
PLANX0896 / 99111
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.