MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Universal Wire Works ER320LR Stainless Steel Bare Wire
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: This alloy has the same basic composition as ER320; however, the elements C, Si, P, and S are specified at lower maximum levels and the Cb and Mn are controlled at narrower ranges. These changes reduce the weld metal hot cracking and fissuring (while maintaining the corrosion resistance) frequently encountered in fully austenitic stainless steel weld metal. Consequently, welding conditions typically used for austenitic stainless steel weld metals containing ferrite can be used in MIG, TIG and submerged-arc applications. ER320LR has a lower minimum tensile strength than ER320 weld metal.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesOriginal ValueComments
Chromium, Cr 20 %
Copper, Cu 3.5 %
Iron, Fe 36.5 %As Remainder
Molybdenum, Mo 2.5 %
Nickel, Ni 34 %
Niobium, Nb (Columbium, Cb) 3.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
330 Stainless Steel, annealed strip
330 Stainless Steel
Cast Stainless Steel CT15C, ASTM A351
ATI AllvacĀ® NickelvacĀ® 23 UNS N08020 Specialty Steel

NUWW076 / 19624

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.