MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Syensqo (Solvay Specialty Polymers) Amodel® FC-1150 (L) PPA, 50% glass fiber
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 50% Glass Fiber Reinforced

Material Notes: 50% glass fiber, approved for food applications

Amodel® FC-1150 and FC-1150 L is an FDA compliant, 50% glass fiber reinforced resin designed for high strength and stiffness (and improved demolding properties for the L grades). This combines with its excellent thermal properties, low water absorption and good hydrolytic stability to make it particularly suited for components used in food service and consumer applications such coffee machines and ovens.

- Natural: FC-1150 (L) NT
- Black: FC-1150 (L) BK 946

Applications: Appliances; Housings; Non-specific Food Applications; Plumbing Parts; Pump Parts

Features: Chemical Resistant; Chlorine Resistant; Creep Resistant; Good Dimensional Stability; Good Stiffness; High Stiffness; High Strength; High Temperature Strength; Low Moisture Absorption

Injection notes: Mold Temperature:
- Higher tool temperatures might be required for thin wall sections
- Minimum mold temperature for typical article thickness is 150°C (302°F)
Storage:
- Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Amodel® processing guide.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.67 g/cc0.0603 lb/in³Method A; ISO 1183
Linear Mold Shrinkage, Flow  0.0014 cm/cm
@Thickness 1.00 mm
0.0014 in/in
@Thickness 0.0394 in
ASTM D955
 0.0015 cm/cm
@Thickness 2.00 mm
0.0015 in/in
@Thickness 0.0787 in
ASTM D955
 0.0016 cm/cm
@Thickness 1.00 mm
0.0016 in/in
@Thickness 0.0394 in
ASTM D955
 0.0018 cm/cm
@Thickness 2.00 mm
0.0018 in/in
@Thickness 0.0787 in
ASTM D955
Linear Mold Shrinkage, Transverse  0.0042 cm/cm
@Thickness 1.00 mm
0.0042 in/in
@Thickness 0.0394 in
ASTM D955
 0.0042 cm/cm
@Thickness 2.00 mm
0.0042 in/in
@Thickness 0.0787 in
ASTM D955
 0.0043 cm/cm
@Thickness 2.00 mm
0.0043 in/in
@Thickness 0.0787 in
ASTM D955
 0.0046 cm/cm
@Thickness 1.00 mm
0.0046 in/in
@Thickness 0.0394 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 270 MPa39200 psiISO 527-2
Elongation at Break 2.0 %2.0 %ISO 527-2
Tensile Modulus 19.1 GPa2770 ksiISO 527-2
Flexural Strength 400 MPa58000 psiISO 178
Flexural Modulus 18.4 GPa2670 ksiISO 178
Charpy Impact Unnotched 8.80 J/cm²41.9 ft-lb/in²ISO 179
Charpy Impact, Notched 1.20 J/cm²5.71 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 300 °C572 °FUnannealed, Flatwise; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 310 - 330 °C590 - 626 °F
Middle Barrel Temperature 315 - 330 °C599 - 626 °F
Front Barrel Temperature 325 - 335 °C617 - 635 °F
Melt Temperature 320 - 345 °C608 - 653 °FInjection
Mold Temperature 150 °C302 °F
Drying Temperature 120 °C
@Time 14400 sec
248 °F
@Time 4.00 hour
Moisture Content 0.030 - 0.060 %0.030 - 0.060 %Injection
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack; Natural Color
FormsPellets
ProcessingInjection Molding
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4116 / 279916

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.